Tag Archives: Titanium screw galvanic corrosion

Q: I’m using metric Grade 5 titanium bolts, washers and nuts for automotive application. Since the car will never be exposed to any salt water environments do I need to worry about galvanic corrosion? A: Galvanic corrosion is really only a problem if you have a liquid medium between the … Continue reading →

Posted in Application, Corrosion Resistance, FAQs, Material, Specialty Metal Fasteners | Tagged , , , , , , , , , , , | Leave a comment