Q: I have down hole application containing sour gas and high chloride levels. The temperature the bolts are exposed to is around 150F and I’m having trouble with cracking. I tried Super Duplex 2507 but am still having issues. Any ideas? A: Super Duplex 2507 does provide good resistance to … Continue reading →

Posted in Application, Corrosion Resistance, FAQs, Material, Specialty Metal Fasteners | Tagged , , , , , , , , | Leave a comment

Q: I’ve got in a high pressure sour gas well. We’ve been having trouble with 316 stainless steel components breaking. I need a solution but not sure what to use. A: High pressures and sour gas combined can cause cracking and corrosion in most standard stainless and alloy steels. Depending … Continue reading →

Posted in Application, High Strength | Tagged , , , , , , | Leave a comment

Q: I’m running a steam surface condenser which is installed on a steam turbine in a thermal power station. I’m using sea water that could be contaminated with chemical pollutants cooling water side of the condenser. Any ideas on a good fastener for the tubes and water boxes? A: Duplex 2205 … Continue reading →

Posted in Application, Corrosion Resistance, FAQs, High Temperature Resistance, Specialty Metal Fasteners | Tagged , , , , , , , , , , , , | Leave a comment

Q: I’m working on a on a geothermal energy drilling project. Carbon steel we’re currently using to bolt drilling components is failing from corrosion. We have corrosive an environment with high levels of sulfur and salt, as well as temperatures to 260C. Any suggestions? A: Super Duplex 2507 is often used … Continue reading →

Posted in Application, Corrosion Resistance, FAQs, Specialty Metal Fasteners | Tagged , , , , , , , , , , , , , | Leave a comment

Q: I have a waste water purifying situation where I’m using chlorine to treat the water. In addition to the acidic solution produced the fastener will also experience high loads, so I’m also concerned with stress corrosion cracking. Currently Super Duplex 2507 is not doing the job. Any recommendations on … Continue reading →

Posted in Application, Corrosion Resistance, FAQs, High Strength, Specialty Metal Fasteners | Tagged , , , , , , , , | Leave a comment

Q: We have a pulp & paper digester that is used to cook wood chips in an alkaline solution. The fasteners will be exposed to high temperatures and abrasive conditions. Any suggestions? A: Without knowing the specifics of your process, I can make two general material suggestions. Duplex 2205 fasteners are … Continue reading →

Posted in Application, Corrosion Resistance, FAQs, High Temperature Resistance, Material, Specialty Metal Fasteners | Tagged , , , , , , , , , , , , , | Leave a comment

Inconel fasteners are commonly used for extreme environments and come in various “flavors” depending on the needs of the application. This brief paper will give you a quick comparison of the two most popular grades, Inconel 625 and Inconel 718 to help you choose the best material.

Posted in Blog | Tagged , , , , , , , , , , , , | 1 Comment